DSC 214 Polyma Differential Scanning Calorimeter. Netzsch, Germany

The DSC 214 Polyma delivers a powerful solution for requirements in day-to-day measuring tasks in terms of both hardware and software. It is easy to operate while still providing absolute reliability, making this innovative DSC instrument an ideal tool for the research, development, quality assurance and failure analysis of polymer materials.

תיאור

The New All-Inclusive Product Package for DSC Measurements

Easy-to-use, robust, precise, optimized for everyday use – these are the features of the innovative DSC 214 Polyma. The unique design of this instrument encompasses everything needed for successful DSC investigations – regardless of whether the user is a beginner or an experienced professional. Above all, it is the two new software developments that are setting new standards: AutoEvaluation and Identify. These have the potential to revolutionize DSC analysis.

  • New all-inclusive 360° product package for the characterization of polymers
  • Easier sample preparation than ever before
  • Automated measurement and evaluation

  • Temperature range: 

    -170°C to 600°C

  • Gas controller: 

    Switches for 3 gases included

    MFC for 3 gases, option

  • Technical Resolution:

    0.1 μW

  • Enthalpy precision: 

    ±0.1% for indium and ±0.05% to  ± 0.2% for most samples

  • Specific heat determination: Optional

    Temperature modulation: Optional

  • Gas atmospheres: 

    Inert, oxidizing, static and dynamic operation

  • Cooling device options: 

    • Compressed air cooling (RT to 600°C)
    • IC40 (-40°C to 600°C)
    • IC70 (-70°C to 600°C)
    • LN2 (-170°C to 600°C)
  • Indium Response Ratio:

    > 100 mW/K

    (Related to indium as standard material under measurement conditions typically used for polymer investigation)

  • Heating/Cooling rate: 

    0.001 K/min to 500 K/min

    (Maximum rates depend upon the temperature)